Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.500 - 0.580 W/m-K @Temperature 100 - 100 °C |
3.47 - 4.03 BTU-in/hr-ft²-°F @Temperature 212 - 212 °F |
Average value: 0.540 W/m-K Grade Count:3 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Thermal Conductivity | 0.540 - 0.580 W/m-K | 3.75 - 4.03 BTU-in/hr-ft²-°F | Average value: 0.560 W/m-K Grade Count:3 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Thermal Conductivity | 0.580 - 0.580 W/m-K @Temperature 100 - 100 °C |
4.03 - 4.03 BTU-in/hr-ft²-°F @Temperature 212 - 212 °F |
Average value: 0.580 W/m-K Grade Count:1 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |