Thermal Properties Metric English Comments
Thermal Conductivity 0.586 - 0.669 W/m-K
4.06 - 4.64 BTU-in/hr-ft²-°F
Abatron AboCast/AboCure 4-4/50-17 Casting Epoxy for Tooling
Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLongest pot lifeLarges..
Thermal Conductivity 0.586 - 0.669 W/m-K
4.06 - 4.64 BTU-in/hr-ft²-°F
Abatron AboCast/AboCure 4-4/50-12 Casting Epoxy for Tooling
Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: FastBest rigid, chemical, and hea..
Thermal Conductivity 0.586 - 0.669 W/m-K
4.06 - 4.64 BTU-in/hr-ft²-°F
Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling
Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLong pot lifeLarge cas..