Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast/AboCure
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLong pot lifeLarge castingsLow exothermMain Drawbacks: Very slow for very thin castings (
Physical Properties Metric English Comments
Water Absorption 0.10 - 0.50 %
0.10 - 0.50 %
24-200 hours
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D >= 85
>= 85
Tensile Strength at Break 35.9 MPa
5200 psi
Elongation at Break 3.6 %
3.6 %
Flexural Strength 49.6 MPa
7200 psi
Compressive Strength 86.2 MPa
12500 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.586 - 0.669 W/m-K
4.06 - 4.64 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 65.0 - 70.0 °C
149 - 158 °F
93.0 °C
199 °F
Deflection temperature after post-cure
Processing Properties Metric English Comments
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
1-2 lbs