Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.20 - 1.50 W/m-K | 8.33 - 10.4 BTU-in/hr-ft²-°F | |
Parker Chomerics CHO-BOND 584-208 Conductive Adhesive Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m.. |
|||
Thermal Conductivity | 1.20 - 1.50 W/m-K | 8.33 - 10.4 BTU-in/hr-ft²-°F | |
Parker Chomerics CHO-BOND 584-29 Conductive Adhesive Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m.. |
|||
Thermal Conductivity | 0.600 - 1.50 W/m-K | 4.16 - 10.4 BTU-in/hr-ft²-°F | Average value: 0.786 W/m-K Grade Count:7 |
Overview of materials for Epoxy, Molded, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Thermal Conductivity | 1.10 - 1.50 W/m-K @Temperature 25.0 - 300 °C |
7.63 - 10.4 BTU-in/hr-ft²-°F @Temperature 77.0 - 572 °F |
|
China-Yixing Longly Refractories Cordierite Ceramics (Heat Resistance Ceramics) LONGLY's cordierite ceramics' main crystal phrase is 2MgO-2Al2O2-5SiO2, this composition has low thermal expansion coefficient and excellent thermal shock resistance. Maximum service temperature is.. |