Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 11.4 W/m-K @Temperature 500 °C |
79.1 BTU-in/hr-ft²-°F @Temperature 932 °F |
Perpendicular |
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | RT |
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | RT |
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | RT |
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | RT |
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | RT |
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | RT |
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | RT |
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 0% Cold Worked, Not Aged 0% Cold Worked, Not Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes .. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 15% Cold Worked, Aged 15% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 25% Cold Worked, Aged 25% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 30% Cold Worked, Aged 30% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Thermal Conductivity | 11.4 W/m-K @Temperature 23.0 °C |
79.1 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
|
Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybd.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed + Aged Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Typical aging - 1750°F (954°C)/1 h/AC plus 1325°F (.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
Special Metals INCONEL® Alloy 718 Developed in the early 1960's, IN718 is still considered the material of choice for the majority of aircraft engine components with service temperatures below 1200°F (650°C). Inconel 718 is a.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 10% Cold Worked, Aged 10% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 15% Cold Worked 15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 5% Cold Worked 5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internatio.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 5% Cold Worked, Aged 5% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Inte.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 50% Cold Worked, Aged 50% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 20% Cold Worked, Aged 20% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Thermal Conductivity | 11.4 W/m-K | 79.1 BTU-in/hr-ft²-°F | |
HP Alloys Alloy 718, 25% Cold Worked 25% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |