Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel

Category Metal , Ferrous Metal , Austenitic , Stainless Steel
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name INCOLOY®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybdenum, the alloy offers resistance to both oxidizing and reducing acids and salts. The presence of copper increases its resistance to sulfuric acid. The alloy is used in the chemical and petrochemical processing industry. Alloy tubes are cold worked to high strength levels for downhole service in moderately corrosive deep sour gas wells.Information Provided by Special Metals Corporation
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 80 - 90
80 - 90
Annealed
Hardness, Rockwell C 33
33
Cold Worked
Tensile Strength at Break 500 MPa
72500 psi
Annealed
896 MPa
130000 psi
Cold Worked
Tensile Strength, Yield 214 MPa
31000 psi
Annealed
758 MPa
110000 psi
Cold Worked
Elongation at Break 15 %
15 %
Cold Worked
40 %
40 %
Annealed
Modulus of Elasticity 200 GPa

@Temperature 23.0 °C
29000 ksi

@Temperature 73.4 °F
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 93.0 °C
8.33 µin/in-°F

@Temperature 199 °F
15.9 µm/m-°C

@Temperature 260 °C
8.83 µin/in-°F

@Temperature 500 °F
16.8 µm/m-°C

@Temperature 427 °C
9.33 µin/in-°F

@Temperature 801 °F
Specific Heat Capacity 0.450 J/g-°C

@Temperature 100 °C
0.108 BTU/lb-°F

@Temperature 212 °F
Thermal Conductivity 11.4 W/m-K

@Temperature 23.0 °C
79.1 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 26 - 28 %
26 - 28 %
Copper, Cu 0.60 - 1.4 %
0.60 - 1.4 %
Iron, Fe 29.01 - 40.4 %
29.01 - 40.4 %
Balance
Manganese, Mn <= 2.5 %
<= 2.5 %
Molybdenum, Mo 3.0 - 4.0 %
3.0 - 4.0 %
Nickel, Ni 30 - 34 %
30 - 34 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000990 ohm-cm

@Temperature 23.0 °C
0.0000990 ohm-cm

@Temperature 73.4 °F
Users viewing this material also viewed the following: