Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 118 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 17.0 W/m-K

@Temperature 200 °C
118 BTU-in/hr-ft²-°F

@Temperature 392 °F
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..
Thermal Conductivity 17.0 W/m-K

@Temperature 200 °C
118 BTU-in/hr-ft²-°F

@Temperature 392 °F
Outokumpu SAF 2304® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Thermal Conductivity 17.0 W/m-K

@Temperature 200 °C
118 BTU-in/hr-ft²-°F

@Temperature 392 °F
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Thermal Conductivity 17.0 W/m-K

@Temperature 85.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 150 Pb-In Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
Thermal Conductivity 17.0 W/m-K

@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24
Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me..
Thermal Conductivity 17.0 W/m-K

@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re..
Thermal Conductivity 17.0 W/m-K

@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34
Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t..
Thermal Conductivity 17.0 W/m-K

@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel URANUS® B6 N Multipurpose Austenitic Stainless Steel with PREN = 36
Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t..
Thermal Conductivity 17.0 W/m-K

@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red..
Thermal Conductivity 17.0 W/m-K
118 BTU-in/hr-ft²-°F
DIN EN 821-2
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2
DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications.
Thermal Conductivity 17.0 W/m-K
118 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS280A Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 17.0 W/m-K
118 BTU-in/hr-ft²-°F
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel
Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug..
Thermal Conductivity 17.0 W/m-K

@Temperature 23.0 - 100 °C
118 BTU-in/hr-ft²-°F

@Temperature 73.4 - 212 °F
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel
Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s..
Thermal Conductivity 17.0 W/m-K
118 BTU-in/hr-ft²-°F
China-Yixing Longly Refractories 75 Alumina Ceramic
LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, ..
Thermal Conductivity 17.0 W/m-K

@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34
Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion..
Thermal Conductivity 17.0 W/m-K

@Temperature 400 °C
118 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 725LN Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Thermal Conductivity 17.0 W/m-K

@Temperature 200 °C
118 BTU-in/hr-ft²-°F

@Temperature 392 °F
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Thermal Conductivity 17.0 W/m-K

@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel
Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom..
Copyright © lookpolymers.com All Rights Reserved