Eagle Brass 260 Cartridge Brass, 1/2 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Eagle Brass 260 Cartridge Brass, 1/4 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Eagle Brass 260 Cartridge Brass, 3/4 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Eagle Brass 260 Cartridge Brass, Annealed
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Eagle Brass 260 Cartridge Brass, Extra Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Eagle Brass 260 Cartridge Brass, Extra Spring
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Eagle Brass 260 Cartridge Brass, Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Eagle Brass 260 Cartridge Brass, Spring
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Chicago Extruded Metals BioBrass® UNS C26000 Copper-Zinc Alloy