Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.60 W/m-K | 18.0 BTU-in/hr-ft²-°F | through-plane, 10*10*3mm sample; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive. |
|||
Thermal Conductivity | 2.60 W/m-K | 18.0 BTU-in/hr-ft²-°F | through-plane, 10*10*3mm sample; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 compound |
|||
Thermal Conductivity | 2.60 W/m-K | 18.0 BTU-in/hr-ft²-°F | through-plane, 10*10*3mm sample; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 compound |
|||
Thermal Conductivity | 2.60 W/m-K | 18.0 BTU-in/hr-ft²-°F | |
McDanel Advanced Ceramics MV-HR1 Mullite Mullite (3Al2O3 • 2SiO2) is a refractory oxide material combining low thermal expansion, good mechanical strength, and resilience at elevated temperatures. Mullite is formulated to produce den.. |
|||
Thermal Conductivity | 2.60 W/m-K | 18.0 BTU-in/hr-ft²-°F | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Thermal Conductivity | 2.60 W/m-K | 18.0 BTU-in/hr-ft²-°F | |
Sapco C 221 Steatite Information provided by Sapco. |
|||
Thermal Conductivity | 2.59 W/m-K | 18.0 BTU-in/hr-ft²-°F | |
Cotronics Duralco™ 4703 Adhesive and Tooling Compound High temperature resin reinforced with ceramic and metallic fibers and particles, resulting in high thermal stability. Easily machined to close tolerances and will repair and rebuild worn or cracke.. |
|||
Thermal Conductivity | 2.59 - 2.74 W/m-K | 18.0 - 19.0 BTU-in/hr-ft²-°F | |
Crucible Steel CSM® 6 Tool Steel, AISI A6 CSM 6 is an air hardening tool steel offering moderate wear resistance and toughness. It may be hardened from a low hardening temperature for easy heat treatment.Information provided by Crucible Ind.. |