Information provided by Sapco.
Physical Properties Metric English Comments
Density 2.60 g/cc
0.0939 lb/in³
Open Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Mohs 7.0
7.0
Tensile Strength, Ultimate 75.0 MPa
10900 psi
Modulus of Elasticity 80.0 GPa
11600 ksi
Flexural Strength 120 MPa
17400 psi
Compressive Strength 800 MPa
116000 psi
Thermal Properties Metric English Comments
CTE, linear 7.00 µm/m-°C

@Temperature 20.0 °C
3.89 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.900 J/g-°C
0.215 BTU/lb-°F
Thermal Conductivity 2.60 W/m-K
18.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1200 °C
2190 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Dielectric Constant 5.0

@Frequency 1e+6 Hz
5.0

@Frequency 1e+6 Hz
Dielectric Strength 13.0 kV/mm
330 kV/in
AC
Dissipation Factor 0.00062

@Frequency 1e+6 Hz
0.00062

@Frequency 1e+6 Hz
Dielectric Loss Index 250
250