Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 19.0 - 20.5 W/m-K @Temperature 100 - 100 °C |
132 - 142 BTU-in/hr-ft²-°F @Temperature 212 - 212 °F |
Average value: 19.5 W/m-K Grade Count:3 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |