Thermal Properties Metric English Comments
Thermal Conductivity 201 W/m-K

@Temperature 20.0 - 400 °C
1390 BTU-in/hr-ft²-°F

@Temperature 68.0 - 752 °F
Hogen Durakut H15W 68 Tungsten/32 Copper PM Metal Composite
RWMA Class ECM-EDMDURAKUT Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Che..
Thermal Conductivity 201 W/m-K

@Temperature 20.0 - 400 °C
1390 BTU-in/hr-ft²-°F

@Temperature 68.0 - 752 °F
Hogen Duralloy H5W 70 Tungsten/30 Copper PM Metal Composite
RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is ..
Thermal Conductivity 200 - 210 W/m-K
1390 - 1460 BTU-in/hr-ft²-°F
z direction
MarkeTech Cu/Mo/Cu 1:2:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
Thermal Conductivity 200 - 220 W/m-K
1390 - 1530 BTU-in/hr-ft²-°F
MarkeTech Mo60Cu Moly/Copper Heat Sink Material
MoCu alloys are made by sintering molybdenum and copper together. This results in a heat sink of lower density than tungsten-based materials, low thermal expansion, and excellent thermal conductivit..
Thermal Conductivity 200 - 220 W/m-K
1390 - 1530 BTU-in/hr-ft²-°F
MarkeTech W80Cu Tungsten/Copper Heat Sink Material
WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c..
Thermal Conductivity 200 - 220 W/m-K
1390 - 1530 BTU-in/hr-ft²-°F
MarkeTech WCu20 Tungsten Copper Alloy
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Materion Beryllium Copper Alloy 10 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Materion Beryllium Copper Alloy 10 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17500)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Materion Beryllium Copper Alloy 10 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Materion Beryllium Copper Alloy 10 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17500)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Materion Beryllium Copper Alloy 10 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Materion Beryllium Copper Alloy 10 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Materion Beryllium Copper Alloy 10 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Materion Beryllium Copper Alloy 10 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: 2 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Thermal Conductivity >= 200 W/m-K
>= 1390 BTU-in/hr-ft²-°F
Minimum
Materion E20 Beryllium/BeO Composite, 20 Volume% BeO
Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
x-y directions
MMCC Aluminum/Graphite Fiber GA 7-230 Metal Matrix Composite
Discontinuous graphite fiber aluminum product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plate..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
z direction
MMCC Copper/Graphite Fiber GC 7-340 Metal Matrix Composite
Discontinuous graphite fiber copper product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plated,..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Microplasmic Anodizing [Ceramic Coating] for Aluminum, Magnesium, Titanium, Zirconium & Composites
Microplasmic Process is for all types of aluminum, magnesium, titanium and zirconium alloys and composite materials.  It is an electrochemical  micro arc oxidation process for which a U.S. pat..
Thermal Conductivity >= 200 W/m-K
>= 1390 BTU-in/hr-ft²-°F
H.C. Starck MoCu 65/35 Molybdenum-Copper Composite Material
Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
ASTM E1461
M Cubed Technologies HSC-702 Aluminum-toughened Reaction Bonded Silicon Carbide
High fracture tougness reaction bonded SiC. Used in applications that require both high wear and high impact resistance. Bullnoses, fan liners, hydrocyclone liners, etc.Information provided by M C..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
UCAR Carbon UCAR® SF75 Extruded Graphite
Typical uses for extruded grades are in the production of molds and crucibles, heating elements and furnace furniture, liquid metal processing equipment and chemical process equipment.Tabular proper..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Temper T651
Constellium DOKIMA® Rolled Plate Aluminum
DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct..
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Ceradyne CeraTrex™ SC-P2 Silicon Carbide
Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Ceradyne CeraTrex™ SC-P3 Silicon Carbide
Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
AA 5005
Aleris 55HX® Aluminum (5005-H14)
Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ..
Copyright © lookpolymers.com All Rights Reserved