Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 29.0 W/m-K @Temperature 1000 °C |
201 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Thermal Conductivity | 29.0 W/m-K @Temperature 1000 °C |
201 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Thermal Conductivity | 29.0 W/m-K @Temperature 85.0 °C |
201 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 205 In-Pb Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Thermal Conductivity | 29.0 W/m-K | 201 BTU-in/hr-ft²-°F | |
McDanel Advanced Ceramics AP 35 99% Alumina Information provided by McDanel Advanced Ceramic Technologies |
|||
Thermal Conductivity | 29.0 W/m-K @Temperature 20.0 °C |
201 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel CLC 1.2738 Prehardened Mold Steel (300HB/30HRC) for Thick Sections Description: CLC 1.2738 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, Nickel carbon and manganese additions are optimized to have a fully .. |
|||
Thermal Conductivity | 29.0 W/m-K | 201 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS185 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 29.0 W/m-K | 201 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS226 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 29.0 W/m-K | 201 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS235 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 29.0 W/m-K | 201 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS310 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 29.0 W/m-K | 201 BTU-in/hr-ft²-°F | Based on Thermal Resistance Data: R = L x K<sup>-1</sup>x A<sup>-1</sup> |
Epoxy Technology EPO-TEK® H20E-MP Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-MP is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al.. |
|||
Thermal Conductivity | 29.0 W/m-K | 201 BTU-in/hr-ft²-°F | Based on Thermal Resistance Data: R = L x K<sup>-1</sup>x A<sup>-1</sup> |
Epoxy Technology EPO-TEK® H20E Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also .. |
|||
Thermal Conductivity | 29.0 W/m-K @Temperature 399 °C |
201 BTU-in/hr-ft²-°F @Temperature 750 °F |
hardened to 45 HRC |
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel Orvar 2 Microdized is a chromium-molybdenum-vanadium alloyed steelORVAR® 2M / AISI H13 is a conventionally produced hot work tool steel with overall good ductility, toughness, wear resistance, hard.. |
|||
Thermal Conductivity | 29.0 W/m-K @Temperature 20.0 - 100 °C |
201 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Anderman Ceramics EA999 Sintered Alumina, 99.9% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |