Material Notes:
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics of lead-indium as well as good thermal fatigue properties.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 8.52 g/cc
0.308 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 28.6 MPa
4150 psi
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 29.0 W/m-K

@Temperature 85.0 °C
201 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 173 - 181 °C
343 - 358 °F
Solidus 173 °C
343 °F
Liquidus 181 °C
358 °F
Component Elements Properties Metric English Comments
Indium, In 60 %
60 %
Lead, Pb 40 %
40 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000250 ohm-cm
0.0000250 ohm-cm