Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 3.00 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 3.00 - 3.50 W/m-K
20.8 - 24.3 BTU-in/hr-ft²-°F
Through Plane; ASTM E1461
PolyOne Trilliant™ HC HC6200-5001 XR Grey Polyamide 12 (Nylon 12)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Thermal Conductivity 3.00 W/m-K
20.8 BTU-in/hr-ft²-°F
ASTM D5470
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Thermal Conductivity 3.00 W/m-K
20.8 BTU-in/hr-ft²-°F
ASTM D5470
Parker Chomerics THERM-A-GAP™ GEL 8010 High Performance Fully Cured Dispensable Gel
Description: Parker Chomerics fully cured dispensable GELs eliminate time consuming hand assembly, decreasing installation costs and reducing customer manufacturing and purchasing (logistical) compl..
Thermal Conductivity 3.00 W/m-K
20.8 BTU-in/hr-ft²-°F
Silicone property; ASTM E1530
Arlon Thermabond® R37340X008 Primerless Electronic Adhesive  (discontinued **)
Liner: 1 mil FEP; Product: uncured Silicone Rubber; Carrier: 3 mil PTFE coated fiberglas
Thermal Conductivity 3.00 W/m-K
20.8 BTU-in/hr-ft²-°F
GBC L3 Steatite
Ideal for high frequency, low loss, high voltage insulation. Much less expensive than alumina insulatorsApplications: resistor forms, surge arrestors, standoffs, spacers, and coil forms.Machinabili..
Thermal Conductivity 3.00 W/m-K
20.8 BTU-in/hr-ft²-°F
DIN EN 821-2
CeramTec ZN 40 Zirconia, ZrO2-MgO
ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma..
Thermal Conductivity 3.00 W/m-K

@Temperature 100 °C
20.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E 1530
Arlon Thermabond® 99A90X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Thermal Conductivity 3.00 W/m-K
20.8 BTU-in/hr-ft²-°F
Silicone Property; ASTM E 1530
Arlon Thermabond® 99A90N008 Primerless Electronic Adhesive  (discontinued **)
Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.
Copyright © lookpolymers.com All Rights Reserved