Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 3.05 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.440 W/m-K
3.05 BTU-in/hr-ft²-°F
Quadrant EPP Fluorosint® 207 PTFE, Compression Molded Synthetic Mica-filled PTFE (ASTM Product Data Sheet)
Thermal Conductivity 0.440 W/m-K
3.05 BTU-in/hr-ft²-°F
ASTM C177
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade
Amber pelletsInformation provided by Infinite Polymer System II.
Thermal Conductivity 0.440 - 0.770 W/m-K
3.05 - 5.34 BTU-in/hr-ft²-°F
Average value: 0.683 W/m-K Grade Count:4
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi..
Thermal Conductivity 0.440 - 0.620 W/m-K

@Temperature 100 - 100 °C
3.05 - 4.30 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.510 W/m-K Grade Count:14
Overview of materials for Phenolic, Novolac, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values..
Thermal Conductivity 0.440 - 0.440 W/m-K

@Temperature 100 - 100 °C
3.05 - 3.05 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.440 W/m-K Grade Count:1
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..
Thermal Conductivity 0.440 W/m-K

@Temperature 200 °C
3.05 BTU-in/hr-ft²-°F

@Temperature 392 °F
Sharadaa Ceramics Resin Bonded Mattresses
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Thermal Conductivity 0.440 W/m-K

@Temperature 100 °C
3.05 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 4485 Phenolic, Granular, Compression Molded
PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a..
Thermal Conductivity 0.440 W/m-K

@Temperature 100 °C
3.05 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 4548 Phenolic, Granular, Transfer Molded
PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai..
Thermal Conductivity 0.440 W/m-K

@Temperature 100 °C
3.05 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 5482 Phenolic, Granular, Injection Molded
PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect..
Thermal Conductivity 0.440 W/m-K

@Temperature 100 °C
3.05 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 6582 Phenolic, Briquette, Injection Molded
PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo..
Thermal Conductivity 0.440 W/m-K
3.05 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy
Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind..