Thermal Conductivity 44.0 W/m-K

@Temperature 85.0 °C
305 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy 130 Tin-Lead Solder Alloy
Inexpensive utility solderInformation Provided by Indium Corporation
Thermal Conductivity 44.0 W/m-K

@Temperature 85.0 °C
305 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 183 Au-Ge Solder Alloy
Eutectic die attach.Information provided by the manufacturer, Indium Corporation.
Thermal Conductivity 44.0 W/m-K
305 BTU-in/hr-ft²-°F
Special Metals Nickel 212
Wrought nickel strengthened with an added manganese. Used for electrical and electronic applications such as lead wires, supporting components in lamps and cathode-ray tubes, and electrodes in glow..
Thermal Conductivity 44.0 W/m-K
305 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS238 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 44.0 W/m-K
305 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS361 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 44.0 W/m-K
305 BTU-in/hr-ft²-°F
Goodfellow Gold 88/Germanium 12 Eutectic Alloy
Special purpose solder.Information provided by Goodfellow.