Williams Advanced Alloys WS238 Solder

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy , Tin Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS238 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 9.28 g/cc
0.335 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 37.2 MPa
5400 psi
Thermal Properties Metric English Comments
CTE, linear 24.7 µm/m-°C

@Temperature 20.0 °C
13.7 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 44.0 W/m-K
305 BTU-in/hr-ft²-°F
Melting Point 183 - 238 °C
361 - 460 °F
Solidus 183 °C
361 °F
Liquidus 238 °C
460 °F
Component Elements Properties Metric English Comments
Lead, Pb 60 %
60 %
Tin, Sn 40 %
40 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001703 ohm-cm
0.00001703 ohm-cm