Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 38.0 W/m-K @Temperature 85.0 °C |
264 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 204 In-Pb Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion FormaMet, EquaCast® Aluminium Bronze Cold Working Die Alloy FormaMet is an aluminum bronze cold working die alloy used for the drawing or forming of stainless steel, low carbon steel and other materials. When used for deep drawing and forming applications of.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion ToughMet® T3 AT110 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion ToughMet® T3 AT120 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion ToughMet® T3 AT120 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion ToughMet® T3 AT90 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion ToughMet® T3 CA ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion ToughMet® T3 CX105 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Industeel Superplast® 350 Mold Steel SUPERPLAST® 350 offers improved machinability, improved consistency and weldability, improved thermal conductivity, with a higher hardness allowing better mechanical properties and polishability... |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Industeel Superplast® 400 High Hardness Mold Steel SUPERPLAST® 400 is an injection plastic mold steel pre-hardened to a high level of hardness. It is delivered at a typical hardness of 125 kg/mm2. This steel is specially adapted for heavy-duty .. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion ToughMet® T3 CX90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS174 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Goodfellow Platinum 90/Rhodium 10 Thermocouple Alloy The positive element of the type S thermocouple. Type S thermocouples are characterized by a high degree of chemical inertness and stability at high temperatures. Often used as a standard for calibr.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion ToughMet® T3 AT110 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion ToughMet® T3 AT90 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Thermal Conductivity | 38.0 W/m-K | 264 BTU-in/hr-ft²-°F | |
Materion ToughMet® T3 CX105 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |