Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable 3311-xx23D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable W1104L-xx60FRDUV Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable W1604L-xx07FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable WJJC31L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable WJLF112L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous (GTP 50% Tensile); IEC 60216 |
PolyOne Bergamid™ B70 UF V2 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 75.0 - 210 °C | 167 - 410 °F | Average value: 151 °C Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Relative Thermal Index; UL746 |
Matrixx Group 84S7301 Flame Retardant 30% Glass Reinforced PET (V0)
(discontinued **) Data provided by The Matrixx Group, formerly RePlas. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | 70-80°C (160-175°F) Heat distortion temperature. |
Abatron AboWeld 8012-4/AboCure 8012-4 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. A "Woodepox" version. neutral or colored; Low shrinkage. Shelf life is 12+ months.Processing: Pot life: 30-40 minutes. 1/1 ratio. Filled.Applicatio.. |
|||
Maximum Service Temperature, Air | 75.0 - 85.0 °C | 167 - 185 °F | Softening Range |
Huntsman Araldite GT 9654 Bisphenol A Epoxy Solid Resin Weight per Epoxide (EEW, g/eq) 500 to 562. Max color is 1.Comments/Applications: Unmodified bis A "Type 2" epoxy resin. More uniform, higher flow GT 7072-type for use in powder coatings and genera.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
LATI Lastilac 10 ABS/PC ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
LATI Latan 2 POM Polyoxymethylene (POM). Unfilled. High viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
LATI Latan 23UV POM Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 126 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Good UV Resistance; Sunlight Resistant (720 hours) Uses: Cable Jacketing; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL QMTT2 .E73402 Forms: PelletsI.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 4130 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Features: Good UV Resistance; Sunlight Resistant (720 hours) Uses: Flexible Cord Jacketing Forms: Pellets Agency Ratings: UL QMTT2 .E73402 Wire Types: SJTW; STW.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 65005 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Features: Flame Retardant Uses: Communication Wire Jacketing Forms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; .. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 65016 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | 20,000 hours; 50% Tensile Strength; IEC 216; DIN 53446 |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) at 50% RH Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
ELASTO UK Dryflex® 400801S SBS Based Material, 80A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
ELASTO UK Dryflex® 400901S SBS Based Material, 90A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
ELASTO UK Dryflex® 420351S SBS Based Material, 35D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | 70-80°C (160-175°F) Heat distortion temperature. |
Abatron AboWeld 8101-5/AboCure 8101-5 Epoxy Data provided by the manufacturer, Abatron, Inc. 5-minute epoxy thixotropic paste. Vaseline like consistency of 8012-9. Light Amber color. Shelf life is 12+ months.Processing: 1/1 ratio. Pot life:.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Deflection Temp at unknown load |
Abatron AboCast 7703-21/AboCure 7703-21 (A) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRDA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | ASTM D 3575 |
Eurofoam Porocell POR 300/100 Ethylene Octane Metallocene EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Maximum Service Temperature, Air | 75.0 - 140 °C | 167 - 284 °F | Average value: 115 °C Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable W1802L-xx17FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |