Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ P391SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Maximum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ P392SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |