Polymer Property : Maximum Service Temperature, Air = -80.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -62.2 °C
-80.0 °F
Monmouth Rubber & Plastics Durafoamâ„¢ P391SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Maximum Service Temperature, Air -62.2 °C
-80.0 °F
Monmouth Rubber & Plastics Durafoamâ„¢ P392SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..