Material Notes:
Note 1: The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ inch thick sheets. These test pieces were exposed for 120 hours to a cycle consisting of: 1. Light at 70°C for 8 hours 2. Dark at 50° C for 4 hours 3. Condensation Cooling for 15 minutesInformation provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Density 0.240 g/cc
0.00868 lb/in³
Water Absorption <= 1.0 %
<= 1.0 %
ASTM D1056
Linear Mold Shrinkage <= 0.017 cm/cm
<= 0.017 in/in
Note 1
Mechanical Properties Metric English Comments
Tensile Strength >= 1.03 MPa
>= 150 psi
Elongation at Break >= 200 %
>= 200 %
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Compression Set <= 25 %
<= 25 %
B2 – 50%
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -62.2 °C
-80.0 °F
Descriptive Properties Value Comments
Color Black