Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1090 °C | 1990 °F | Sustained |
Pyrotek Dense Fused Silica Pre-Cast Shapes Pyrocast Dense Fused Silica is an economical product for shapes demanding thermal shock resistance at temperatures. Pyrocast DFS stands up to repeated use in molten metal casting in aluminum, coppe.. |
|||
Maximum Service Temperature, Air | 1090 °C | 1990 °F | Continuous |
Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting Vacuum formed shapes are manufactured from high purity alumina silica fibers in one-piece design that eliminates metal leakage. No pre-heating required. Reusable, with proper treatment, for multip.. |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | Use Limit |
Mid-Mountain Materials THERMOSEAL® 2000 High Temperature Cement Description: A family of high temperature resistant cements carefully formulated to withstand thermal expansion and contraction under fluctuating heat conditions. THERMOSEAL® THERMAL CEMENTS are .. |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | Use Limit |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M100 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | |
Cotronics Resbond™ 952 High Temperature Ceramic Adhesive, Nickel Composition |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | |
Cotronics Resbond™ 954 High Temperature Ceramic Adhesive, Stainless Steel Composition |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | Continuous |
Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled This coating system, originally patented by Aremco, is a tow-part, silica-bonded, titanium diboride filled, oxidation resistant coating for protecting graphite from oxidation to 2000°F (1093°C). U.. |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | |
Aremco Pyro-Putty™ 653 High Temperature Ceramic-Metallic Putty, Stainless Filled Ceramic and Stainless-Filled, One-Part, Water Based Paste.For Vertical Surfaces and Applications to 1/2" Thick.Repairs Cast Iron, Steel and Stainless Parts to 2000°F. |
|||
Maximum Service Temperature, Air | 1090 °C | 1990 °F | |
Pyrotek ZP2500 Fabric Splash guards, thick curtains, tadpoles, tapesInformation provided by Pyrotek. |