Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1090 °C | 2000 °F | Use Limit |
Mid-Mountain Materials THERMOSEAL® 2000 High Temperature Cement Description: A family of high temperature resistant cements carefully formulated to withstand thermal expansion and contraction under fluctuating heat conditions. THERMOSEAL® THERMAL CEMENTS are .. |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | Use Limit |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M100 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | |
Cotronics Resbond™ 940 High Temperature Ceramic Adhesive, Fast Set |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | |
Cotronics Resbond™ 954 High Temperature Ceramic Adhesive, Stainless Steel Composition |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | |
Aremco Ceramabind™ 830 High Temperature Inorganic Binder A basic solution compatible with most oxide and metal powders. Ideal for formulating high pigment-to-binder ratios to produce dense adhesives and coatings. Sets at room temperature to a moisture res.. |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | Continuous |
Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled This coating system, originally patented by Aremco, is a tow-part, silica-bonded, titanium diboride filled, oxidation resistant coating for protecting graphite from oxidation to 2000°F (1093°C). U.. |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | |
Aremco HiE-Coat™ 840-M High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for carbon and stainless steel to 2000 °F (1093°C). |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | |
Aremco Pyro-Putty™ 2400 High Temperature Ceramic-Metallic Putty, Stainless Filled Ceramic and Stainless-Filled, One-Part, Water Based Paste.For Applications to 3/8" Thick.Repairs Cast Iron, Steel and Stainless Parts to 2000°F |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | |
Aremco Pyro-Putty™ 653 High Temperature Ceramic-Metallic Putty, Stainless Filled Ceramic and Stainless-Filled, One-Part, Water Based Paste.For Vertical Surfaces and Applications to 1/2" Thick.Repairs Cast Iron, Steel and Stainless Parts to 2000°F. |
|||
Maximum Service Temperature, Air | 1090 °C | 2000 °F | Continuous |
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps.. |