Polymer Property : Maximum Service Temperature, Air = 200 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 - 93.3 °C
158 - 200 °F
Average value: 75.1 °C Grade Count:14
Overview of materials for PVC, Foam Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma..