Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco HiE-Coat™ 840-M High Emissivity Coating, Inorganic-Ceramic Filled

Category Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Aremco
Trade Name HiE-Coat™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco HiE-Coat™ 840-M High Emissivity Coating, Inorganic-Ceramic Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ceramic-based, black-pigmented coating for carbon and stainless steel to 2000 °F (1093°C).
Physical Properties Metric English Comments
Density >= 1.54 g/cc
>= 0.0556 lb/in³
Solids Content 46.3 %
46.3 %
by volume
50.0 %
50.0 %
by weight
Volatile Organic Compounds (VOC) Content 0.000 g/l
0.000 g/l
Viscosity 600 - 900 cP
600 - 900 cP
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
53.8 microns
2.12 mil
estimated wet film thickness
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1090 °C
2000 °F
Processing Properties Metric English Comments
Processing Temperature 50.0 - 90.0 °C
122 - 194 °F
Application Temp
Cure Time 60.0 min

@Temperature 93.3 °C
1.00 hour

@Temperature 200 °F
Step 1, preceeded by 1 hour air set
60.0 min

@Temperature 260 °C
1.00 hour

@Temperature 500 °F
Step 2
Shelf Life 6.00 Month

@Temperature 12.8 - 29.4 °C
6.00 Month

@Temperature 55.0 - 85.0 °F
Descriptive Properties Value Comments
Color Jet Black
Dry Film Coverage ft2/gal 742
at 1 mil
Thinner 840M-T