Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 200 - 240 °C | 392 - 464 °F | Average value: 229 °C Grade Count:28 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Maximum Service Temperature, Air | 180 - 240 °C | 356 - 464 °F | Average value: 228 °C Grade Count:22 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Maximum Service Temperature, Air | 200 - 240 °C | 392 - 464 °F | Average value: 224 °C Grade Count:16 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | Average value: 230 °C Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Maximum Service Temperature, Air | 90.0 - 240 °C | 194 - 464 °F | Average value: 154 °C Grade Count:7 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Maximum Service Temperature, Air | 90.0 - 240 °C | 194 - 464 °F | Average value: 154 °C Grade Count:36 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Maximum Service Temperature, Air | 115 - 240 °C | 239 - 464 °F | Average value: 155 °C Grade Count:4 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | UL Temperature Rating |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | UL Temperature Rating |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | UL Temperature Rating |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | UL Temperature Rating |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | UL Temperature Rating |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | UL Temperature Rating |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | UL Temperature Rating |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |