Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 399 °C @Pressure 10.3 MPa |
750 °F @Pressure 1500 psi |
Continuous |
Garlock 706 Compressed Inorganic Fiber Gasketing, Nitrile Binder Inorganic fibers with a nitrile binder.Inorganic, asbestos-free fibers offer superior performance in saturated and superheated steamThermally stable fibers retain effective seal even during thermal .. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | Short Term |
Mid-Mountain Materials HYTEX® 700 Kevlar® Glass Industrial Textile Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemi.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | In oxygen |
SGL Carbon Group EK 10 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | In oxygen |
SGL Carbon Group EK 17 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | In oxygen |
SGL Carbon Group EK 20 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | In oxygen |
SGL Carbon Group EK 2209 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | In oxygen |
SGL Carbon Group EK 2239 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | In oxygen |
SGL Carbon Group EK 24 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | In oxygen |
SGL Carbon Group EK 3105 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | In oxygen |
SGL Carbon Group EK 3205 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | In oxygen |
SGL Carbon Group EK 3235 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | In oxygen |
SGL Carbon Group EK 3245 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 399 °C | 750 °F | |
Aremco AREMCOLOX™ 502-400 Machinable Glass Ceramic High dielectric and mechanical strength. For high voltage insulators, coil forms, soldering fixtures, arc barriers. Readily machined, no firing required. Plates from 1/8" to 1" thick; rods from 1.. |