Polymer Property : Maximum Service Temperature, Air = 40.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 40.0 °C
104 °F
Abatron 82093 A/B Filled Potting Compound  (discontinued **)
Gray filled epoxy to bond new to old concrete and other surfaces. 1/1 ratio.Information provided by Abatron.
Maximum Service Temperature, Air 40.0 °C
104 °F
Abatron UWBONDL A/B Filled Potting Compound  (discontinued **)
Filled epoxy to bond dry, wet, or underwater. 1/1 ratio.Information provided by Abatron.
Maximum Service Temperature, Air 40.0 °C
104 °F
Karina CAK 65-48/1 Black PVC Compound
Reclaimed PVC compound recommended for soles and general purpose injected articles (whose temperature of use do not exceed 40°C).Information provided by Karina Indústria e Comércio de Plá..
Maximum Service Temperature, Air 40.0 °C
104 °F
Henkel Frekote 915WB Mold Cleaner
A water-based cleaner for composite and metal molds. The surfactants and emulsifiers in combination with soft abrasives give excellent cleaning results without dulling or scratching the surface.Bene..
Maximum Service Temperature, Air 40.0 °C
104 °F
Henkel Frekote PMC Mold Solvent
PMC is a special blend of solvents designed to dissolve and remove wax from molds without dulling the surface. This product can also be used to clean composite and metal mold surfaces as well as for..
Maximum Service Temperature, Air 40.0 °C
104 °F
Wet Service (Continuous)
Chesterton ARC CS4 low-viscosity, 100% solids, barrier coating
Description: An advanced composite formulated to protect concrete surfaces from harsh chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat in a 2 coat syst..
Maximum Service Temperature, Air <= 40.0 °C
<= 104 °F
Laundering Resistance
EMS-Griltech Griltex® D 1299A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Maximum Service Temperature, Air <= 40.0 °C
<= 104 °F
Laundering Resistance
EMS-Griltech Griltex® D 1365E Copolyester Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Maximum Service Temperature, Air <= 40.0 °C
<= 104 °F
Laundering Resistance
EMS-Griltech Griltex® D 1666A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Maximum Service Temperature, Air 40.0 - 60.0 °C
104 - 140 °F
long term; EMS
EMS-Grivory Grivory® GTR 45 PA6I/6T
Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides..
Maximum Service Temperature, Air 40.0 °C
104 °F
continuous
CENTROPLAST BC NF Organic Thermoplastic, 15% Natural Fiber
CENTROPLAST BC NF 15 is made of CO2-neutral, sustainable raw-materials with 15% natural fiber.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegr..
Maximum Service Temperature, Air 40.0 - 100 °C
104 - 212 °F
Average value: 52.4 °C Grade Count:30
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Maximum Service Temperature, Air 40.0 °C
104 °F
continuous
CENTROPLAST BC Organic Thermoplastic
CENTROPLAST BC is made of CO2-neutral, sustainable raw-materials.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegradable by composting accordin..