Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CENTROPLAST BC Organic Thermoplastic

Category Polymer , Renewable/Recycled Polymer , Thermoplastic
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST BC Organic Thermoplastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CENTROPLAST BC is made of CO2-neutral, sustainable raw-materials.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegradable by composting according to DIN EN 13432. Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Moisture Absorption 0.500 %

@Temperature 23.0 °C
0.500 %

@Temperature 73.4 °F
normal humidity; ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
Tensile Strength 22.7 MPa
3290 psi
5 mm/min; ISO 527-2
Elongation at Break 11.8 %
11.8 %
ISO 527-2
Tensile Modulus 2.74 GPa
397 ksi
ISO 527-2
Flexural Modulus 1.82 GPa
264 ksi
ISO 178
Charpy Impact Unnotched 5.80 J/cm²
27.6 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 152 °C
306 °F
DSC, 10 K/m; ISO 3146
Maximum Service Temperature, Air 40.0 °C
104 °F
continuous
58.0 °C
136 °F
short term
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ISO 75-2
Vicat Softening Point 58.0 °C
136 °F
VST/B/50; ISO 306
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Descriptive Properties Value Comments
Color White
Food Compliance BfR: Yes
Food Compliance FDA Yes