Thermal Properties Metric English Comments
Maximum Service Temperature, Air 350 - 450 °C
662 - 842 °F
Cellulosics, Polyolefins, Styrenics & PVC Resins
Claude Bamberger Ultimax® 9100 Purge Compound
Ultimax® is recommended for ABS, nylon, polycarbonate, PET, and other high temperature engineering plastics. Temperature range 350-525°F (176-275°C). Ultimax® 9100 is environmentally friendlie..