Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs S20 ABS Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs SS0 GK10 ABS, High Flow Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 45FS GKF2010 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANLON A 5005 PA/ABS-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANLON A 5005B PA/ABS-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANLON A 5005B UV PA/ABS-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs F00 ABS Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/min; ASTM D1525 |
Kingfa HR-527 Modified ABS Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Vicat Softening Point | 105 °C @Load 1.02 kg |
221 °F @Load 2.25 lb |
50°C/h; ISO 306 |
Styrolution Luran® S 767KE ASA Luran S 767KE is particular suitable for co-extrusion with PVC at low temperature. Hereby, it provides a glossy surface finish.Enhanced flowabilitySuitable for co-extrusion with PVCEnables high glos.. |
|||
Vicat Softening Point | 105 °C @Load 5.10 kg |
221 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro.. |
|||
Vicat Softening Point | 105 °C @Load 1.02 kg |
221 °F @Load 2.25 lb |
50°C/h; ISO 306 |
Styrolution Terlux® HD 2822 MABS Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well .. |
|||
Vicat Softening Point | 105 °C @Load 5.10 kg |
221 °F @Load 11.2 lb |
ISO 306 |
Borealis PS65C40 Polypropylene Compound, Mineral Filled PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and.. |
|||
Vicat Softening Point | 105 °C @Load 0.999 kg |
221 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND 4500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, excellent mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 105 °C @Load 5.00 kg |
221 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 0417 GIF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 105 °C @Load 5.00 kg |
221 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 3510 HT Acrylonitrile Butadiene Styrene ABS with very high impact resistanceHigh impact resistance at low temperature, high heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 105 °C @Load 0.999 kg |
221 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 3520 Acrylonitrile Butadiene Styrene ABS with high impact resistanceHigh melt flow rate, high impact resistance at low temperature, excellent processability and surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Kibilac® PW-957 ASA Polymer Injection |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Kibisan® PN-106 L150 SAN High Clarity |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Kibisan® PN-107 L125 SAN High Clarity |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-717C ABS Medium impact |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PH-888G Polystyrene - High gloss High impact; high gloss |
|||
Vicat Softening Point | 105 - 110 °C @Load 5.00 kg |
221 - 230 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
Vicat Softening Point | 105 °C @Load 5.00 kg |
221 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-747F ABS - Extrusion Refrigerator |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-757 ABS High gloss, medium impact |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
Vicat Softening Point | 105 °C @Load 5.00 kg |
221 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-777B ABS - High Heat High Heat Impact |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |
|||
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs F00 GF17 ABS, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 5.10 kg |
221 °F @Load 11.2 lb |
50°C/hour; ISO 306 |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |