Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Terlux® HD 2822 MABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Manufacturer Styrolution
Trade Name Terlux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Terlux® HD 2822 MABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well known in SAN molding compositions.Excellent transparencyGood resistance to chemicalsGood Stiffness and surface finishHigh impact strengthHD service package availableInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Water Absorption at Saturation 0.70 %

@Temperature 23.0 °C
0.70 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ISO 294-4
Melt Flow 2.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
2.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
17 g/10 min

@Load 21.6 kg,
Temperature 220 °C
17 g/10 min

@Load 47.6 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Ball Indentation Hardness 70.0 MPa
10200 psi
ISO 2039-1
Tensile Strength, Yield 48.0 MPa
6960 psi
ISO 527
Elongation at Break 12 %
12 %
ISO 527
Elongation at Yield 4.0 %
4.0 %
ISO 527
Tensile Modulus 2.00 GPa
290 ksi
ISO 527
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Charpy Impact Unnotched 8.00 J/cm²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179
12.0 J/cm²

@Temperature 23.0 °C
57.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.200 J/cm²

@Temperature -30.0 °C
0.952 ft-lb/in²

@Temperature -22.0 °F
ISO 179
0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
CTE, linear 80.0 - 110 µm/m-°C
44.4 - 61.1 µin/in-°F
ISO 11359
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75
Vicat Softening Point 93.0 °C

@Load 5.10 kg
199 °F

@Load 11.2 lb
50°C/h; ISO 306
105 °C

@Load 1.02 kg
221 °F

@Load 2.25 lb
50°C/h; ISO 306
Optical Properties Metric English Comments
Refractive Index 1.54
1.54
Sodium D Line; ASTM D 542
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Dielectric Constant 2.9

@Frequency 100 Hz
2.9

@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.014

@Frequency 1.00e+6 Hz
0.014

@Frequency 1.00e+6 Hz
IEC 60250
0.016

@Frequency 100 Hz
0.016

@Frequency 100 Hz
IEC 60250
Processing Properties Metric English Comments
Melt Temperature 230 - 260 °C
446 - 500 °F
ISO 294
Mold Temperature 60.0 °C
140 °F
ISO 294
Injection Velocity 200 mm/sec
7.87 in/sec
ISO 294
Drying Temperature 70.0 °C

@Time >=7200 sec
158 °F

@Time >=2.00 hour
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved