Pyrotek MT-29Q Quilted Microporous Insulation

Category Ceramic , Glass
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek MT-29Q Quilted Microporous Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MT-29Q is quilted to encapsulate its microporous core between glass cloth. The result is a flexible insulating material which offers exceptionally low thermal conductivity. The quilting maintains the core distribution to ensure its insulating effectiveness and provide resistance to vibration.ApplicationsBackup insulation for: Troughs Filter bowls Furnace linings Transfer crucibles Door insulation Curved surfaces Irregular shapes Ladle linings AdvantagesLow thermal conductivity Reduces warping of vessels and troughing Promotes greater temperature control Minimizes heat transfer Can be designed to be reused Minimizes hot face temperature of vessels Provides low shrinkage at high temperatures Not wet by molten aluminum Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.256 g/cc
0.00925 lb/in³
Mechanical Properties Metric English Comments
Compressive Strength 0.200 MPa
29.0 psi
to 10% deformation
0.600 MPa
87.0 psi
to 20% deformation
1.10 MPa
160 psi
to 30% deformation
Thermal Properties Metric English Comments
Thermal Conductivity 0.0290 W/m-K

@Temperature 260 °C
0.201 BTU-in/hr-ft²-°F

@Temperature 500 °F
(Standard and Hydrophobic)
0.0420 W/m-K

@Temperature 537 °C
0.291 BTU-in/hr-ft²-°F

@Temperature 999 °F
Standard
0.0480 W/m-K

@Temperature 537 °C
0.333 BTU-in/hr-ft²-°F

@Temperature 999 °F
(Hydrophobic)
0.0490 W/m-K

@Temperature 649 °C
0.340 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Standard
0.0560 W/m-K

@Temperature 649 °C
0.389 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Hydrophobic
Maximum Service Temperature, Air 650 °C
1200 °F
for Continuous use with standard cloth exterior
1000 °C
1830 °F
for Continuous use with specialty cloth exterior or flexible core
Shrinkage 0.300 %

@Temperature 538 °C
0.300 %

@Temperature 1000 °F
0.600 %

@Temperature 815 °C
0.600 %

@Temperature 1500 °F
1.30 %

@Temperature 954 °C
1.30 %

@Temperature 1750 °F