Thermal Properties Metric English Comments
Thermal Conductivity 0.240 - 0.340 W/m-K

@Temperature 600 °C
1.67 - 2.36 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable
Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati..