Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.240 W/m-K @Temperature 650 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 650 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 315 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 599 °F |
|
Pyrotek ISOMAG® 70 Structural Insulation Isomag® 70 is magnesia silicate based formulation provides insulating properties similar to calcium silicate with good strength and dimensional stability up to 1000°C. ApplicationsTorpedo cars La.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 815 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 1500 °F |
|
Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting Vacuum formed shapes are manufactured from high purity alumina silica fibers in one-piece design that eliminates metal leakage. No pre-heating required. Reusable, with proper treatment, for multip.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 400 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 1650 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 100 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1530 |
3M Dyneon™ CCM605 PTFE, 25% Glass Filled
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 250 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ TFM™ 1600 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Dyneon TFM 1600 PTFE is a free-flowing powder for compression molding, isostatic molding, automatic molding, and ram extrusion. Dyneon™ TFM™ 1600 PTFE is a second-generatio.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 250 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ TR 1105 PTFE
(discontinued **) Ideal for thin wall ram extrusion productsReduces cold flow and melt viscosityLower permeabilityLower porosityWeldableExcellent product smoothnessIncreased machine outputInformation provided by Dyne.. |
|||
Thermal Conductivity | 0.240 - 0.320 W/m-K @Temperature 100 °C |
1.67 - 2.22 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 1.2.4. MIX GM Refractory Insulating Castable Description: This light weight gunning castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Re.. |
|||
Thermal Conductivity | 0.240 - 0.340 W/m-K @Temperature 600 °C |
1.67 - 2.36 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 600 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-201 supplemented by ASTM C-182 |
Skamol Group SKAMOCAST 112-80 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 200 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-201 supplemented by ASTM C-182 |
Skamol Group SKAMOCAST 14-105 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 400 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 1650 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 1093 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 1999 °F |
ASTM C182 |
BNZ Materials BNZ-20 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 1093 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 1999 °F |
ASTM C182 |
BNZ Materials BNZ-23A Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 200 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 392 °F |
ASTM C182 |
BNZ Materials BNZP-26 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 400 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTM C182 |
BNZ Materials Color A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |