Thermal Properties Metric English Comments
Thermal Conductivity 1.10 W/m-K

@Temperature 540 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Pyrotek Pyrocast AR-S Castable Refractory
Pyrocast AR-S is a low cement, fused silica, castable refractory which exhibits excellent resistance to thermal shock. It is inert to liquid aluminum and its alloys. It is a high strength material..
Thermal Conductivity 1.10 W/m-K

@Temperature 100 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast B 1 Dense Refractory Brick
Description: B 1 is a fireclay quality for general applications up to 1350°CRemarks: This data represents average values, obtained from samples that were cut from standard bricks.Information prov..
Thermal Conductivity 1.10 W/m-K

@Temperature 650 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast C Dense Refractory Brick
Description: A dry-pressed fireclay brick for use up to 1250°C with a good resistance to acid slags and vapors. Application: industrial furnaces, chimneys, electrolytic reduction cells.Remarks: T..
Thermal Conductivity 1.10 - 1.30 W/m-K

@Temperature 600 °C
7.63 - 9.02 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 60 S Moldable Refractory Material
Description: Because this material contains a high percentage of sillimanite, it has a very good thermal shock resistance together with a very good slag resistance. Therefore this material finds its..
Thermal Conductivity 1.10 - 1.20 W/m-K

@Temperature 100 °C
7.63 - 8.33 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 160 FS Dense Refractory Castable
Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f..
Thermal Conductivity 1.10 - 1.20 W/m-K

@Temperature 100 °C
7.63 - 8.33 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable
Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.10 - 1.20 W/m-K

@Temperature 100 °C
7.63 - 8.33 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable
Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar..
Thermal Conductivity 1.10 - 1.20 W/m-K

@Temperature 100 °C
7.63 - 8.33 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable
Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.10 W/m-K

@Temperature 650 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast C Sp Dense Refractory Brick
Description: A fireclay brick for use up to 1200°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.10 W/m-K

@Temperature 800 °C,
Time 10800 sec
7.63 BTU-in/hr-ft²-°F

@Temperature 1470 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST K High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Thermal Conductivity 1.10 W/m-K

@Temperature 800 °C,
Time 10800 sec
7.63 BTU-in/hr-ft²-°F

@Temperature 1470 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Thermal Conductivity 1.10 W/m-K

@Temperature 400 °C,
Time 10800 sec
7.63 BTU-in/hr-ft²-°F

@Temperature 752 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST LC60 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Thermal Conductivity 1.10 W/m-K

@Temperature 200 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; EN 993-15 1998
Skamol Group SKAMOBAR 69 Low-Alumina Fireclay Brick
Low-alumina fireclay brick has the following characteristics: Max. service temperature 1100°C (2012°F)For barrier lining of aluminum reduction cellsExcellent cryolite resistanceLow thermal con..