Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name VIBRON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 75.0 - 85.0 MPa

@Temperature 100 °C
10900 - 12300 psi

@Temperature 212 °F
Cold Crushing Strength
100 - 120 MPa

@Temperature 1300 °C
14500 - 17400 psi

@Temperature 2370 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.10 - 1.20 W/m-K

@Temperature 100 °C
7.63 - 8.33 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.13 - 1.23 W/m-K

@Temperature 600 °C
7.84 - 8.54 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.20 - 1.30 W/m-K

@Temperature 1300 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1400 °C
2550 °F
Shrinkage -0.400 - 0.400 %

@Temperature 1300 °C
-0.400 - 0.400 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 47 %
47 %
Fe2O3 1.5 %
1.5 %
SiO2 47 %
47 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 2300 kg
Mixing Water 5.5-6.5 liters
per 100 kgs dry material
Users viewing this material also viewed the following: