Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 10.1 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.46 W/m-K

@Temperature 538 °C
10.1 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Pyrotek Pyrocast ALFS Abrasion-Resistant Refractory Castable
Pyrocast ALFS refractory is a high flow, fused silica castable. At low water levels (6.5-7%), Pyrocast ALFS exhibits outstanding flow characteristics.ApplicationsAluminum melting equipment Aluminum..
Thermal Conductivity 1.45 W/m-K

@Temperature 700 °C
10.1 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Pyrotek Pyrocast 220HT Refractory Castable
Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r..
Thermal Conductivity 1.45 W/m-K

@Temperature 1100 °C
10.1 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 42 Dense Refractory Brick
Description: Because of its abrasion resistance and high density, this brick performs very well in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were c..
Thermal Conductivity 1.45 - 1.65 W/m-K

@Temperature 100 °C
10.1 - 11.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 180 B Dense Refractory Castable
Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can..
Thermal Conductivity 1.45 - 1.65 W/m-K

@Temperature 100 °C
10.1 - 11.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 180 Dense Refractory Castable
Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th..
Thermal Conductivity 1.45 - 1.65 W/m-K

@Temperature 100 °C
10.1 - 11.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 180 TF Dense Refractory Castable
Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark..
Thermal Conductivity 1.45 - 1.55 W/m-K

@Temperature 1400 °C
10.1 - 10.8 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Gouda Vuurvast VIBRON 160 H GS (R) Dense Vibrating Refractory Castable
Description: Vibron 160 H GS (R) is a pumpable low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock-, corrosion- and abrasion resista..
Thermal Conductivity 1.45 - 1.65 W/m-K

@Temperature 600 °C
10.1 - 11.5 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 160 H SiC Dense Vibrating Refractory Castable
Description: Vibron 160 H SiC is a low cement vibrating castable characterized by a high strength, good abrasion resistance and excellent thermal shock resistance. Because of the presence of SiC, th..
Thermal Conductivity 1.45 - 1.65 W/m-K

@Temperature 1400 °C
10.1 - 11.5 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable
Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide..
Thermal Conductivity 1.45 W/m-K

@Temperature 1100 °C
10.1 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast A 1 S Dense Refractory Brick
Description: A brick with a high creep resistance, successfully applied in anode baking furnaces and in the transition zone of rotary cement kilns.Remarks: This data represents average values, obtai..
Thermal Conductivity 1.46 W/m-K

@Temperature 1100 °C
10.1 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 44 Dense Refractory Brick
Description: A very dense, high duty fireclay brick with low iron and alkali content. Widely used in anode-baking furnaces (aluminum industry) and as the lining of the top of blast furnaces.Remarks:..
Thermal Conductivity 1.45 W/m-K

@Temperature 800 °C,
Time 10800 sec
10.1 BTU-in/hr-ft²-°F

@Temperature 1470 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST A High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Thermal Conductivity 1.45 W/m-K

@Temperature 600 °C,
Time 10800 sec
10.1 BTU-in/hr-ft²-°F

@Temperature 1110 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST LC70 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Thermal Conductivity 1.45 - 1.65 W/m-K

@Temperature 100 °C
10.1 - 11.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable
Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply ..
Thermal Conductivity 1.46 W/m-K

@Temperature 1100 °C
10.1 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 45 Dense Refractory Brick
Description: High quality refractory brick with a good volume stability up to 1450°C. Used where high load bearing capacities are required e.g. blast furnace stoves.Remarks: This data represents av..