Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
After drying at 110°C
Particle Size <= 3000 µm
<= 3000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1600 °C
5080 - 6530 psi

@Temperature 2910 °F
Cold Crushing Strength
45.0 - 55.0 MPa

@Temperature 100 °C
6530 - 7980 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.28 - 1.48 W/m-K

@Temperature 600 °C
8.88 - 10.3 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.35 - 1.55 W/m-K

@Temperature 1600 °C
9.37 - 10.8 BTU-in/hr-ft²-°F

@Temperature 2910 °F
1.45 - 1.65 W/m-K

@Temperature 100 °C
10.1 - 11.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1870 °C
3400 °F
Shrinkage -0.500 - 0.500 %

@Temperature 1600 °C
-0.500 - 0.500 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 94 %
94 %
CaO 4.5 %
4.5 %
Fe2O3 0.20 %
0.20 %
SiO2 0.20 %
0.20 %
Descriptive Properties Value Comments
ASTM Classification G
Material Consumption per 1 m3 2700 kg
Mixing Water 8-10 liters
per 100 kgs dry material