Thermal Conductivity 2.45 - 2.55 W/m-K

@Temperature 600 °C
17.0 - 17.7 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 90 Moldable Refractory Material
Description: This high refractory ramming material contains several well defined corundum qualities and only a small quantity of binding agent. Curas 90 has a very good resistance against erosion an..
Thermal Conductivity 2.45 W/m-K

@Temperature 316 °C
17.0 BTU-in/hr-ft²-°F

@Temperature 600 °F
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19
Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance..
Thermal Conductivity 2.45 W/m-K

@Temperature 316 °C
17.0 BTU-in/hr-ft²-°F

@Temperature 600 °F
Crucible Steel PEERLESS A Tool Steel, AISI H21
Peerless A is designed for tools which will run hot, at operating temperatures between about 600F and 1100F. The tools should not be water cooled in service, due to a high risk of thermal shock. Pee..