Polymer Property : Thermal Conductivity = 17.7 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 2.45 - 2.55 W/m-K

@Temperature 600 °C
17.0 - 17.7 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 90 Moldable Refractory Material
Description: This high refractory ramming material contains several well defined corundum qualities and only a small quantity of binding agent. Curas 90 has a very good resistance against erosion an..