Thermal Properties Metric English Comments
Thermal Conductivity 0.290 W/m-K

@Temperature 538 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Pyrotek NAD-1000 High Temperature Engineering Board
NAD-1000 is a high density calcium silicate board reinforced with selected fibers to produce excellent thermal characteristics and dimensional stability up to 1000°C. NAD-1000 retains high strengt..
Thermal Conductivity 0.290 W/m-K

@Temperature 23.0 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Average; ISO/CD 22007-4
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
Thermal Conductivity 0.290 W/m-K

@Temperature 100 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled  (discontinued **)
Type I, non-free-flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon ..
Thermal Conductivity 0.290 W/m-K

@Temperature 100 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CC605 PTFE 25% Fiberglass Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.
Thermal Conductivity 0.290 - 0.390 W/m-K

@Temperature 600 °C
2.01 - 2.71 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GI 26 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.290 - 0.390 W/m-K

@Temperature 1200 °C
2.01 - 2.71 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable
Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod..
Thermal Conductivity 0.290 W/m-K

@Temperature 600 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group VIP 12 Vermiculite Insulating Slab
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr..
Thermal Conductivity 0.290 W/m-K

@Temperature 1650 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 3000 °F
Zircar Refractory Composites RS-99-45 Refractory Sheet
ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani..
Thermal Conductivity 0.290 W/m-K

@Temperature 600 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1110 °F
parallel to thickness
Zircar Refractory Composites ZIRCAL-95 Refractory Board
Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for..
Thermal Conductivity 0.290 W/m-K

@Temperature 1093 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1999 °F
8 pcf blanket (Parallel to Thickness)
Zircar Ceramics ASB-2300 Alumina-Silica Blanket
Useful to temperatures of 1260°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics.
Thermal Conductivity 0.290 W/m-K

@Temperature 1093 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1999 °F
8 pcf blanket (Parallel to Thickness)
Zircar Ceramics ASB-2600 Alumina-Silica Blanket
Useful to temperatures of 1400°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics.
Thermal Conductivity 0.291 W/m-K

@Temperature 260 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 500 °F
Chosun Refractories INCT-100N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 0.291 W/m-K

@Temperature 260 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 500 °F
Chosun Refractories INCT135S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 0.290 W/m-K

@Temperature 1093 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials BNZ-23HS Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.290 W/m-K

@Temperature 538 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1000 °F
ASTM C182
BNZ Materials BNZ-26-60 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.290 W/m-K

@Temperature 1000 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1830 °F
ASTM C182
BNZ Materials BNZP-26A Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.290 W/m-K

@Temperature 200 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 392 °F
ASTM C182
BNZ Materials Color CA Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.290 W/m-K

@Temperature 538 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1000 °F
BNZ Materials CS85 High Temperature Structural Insulation
NZ manufactures a variety of non-asbestos calcium silicate structural insulations that combine high strength and excellent thermal insulating characteristics for use in a variety of heat processing,..
Thermal Conductivity 0.290 W/m-K

@Temperature 538 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1000 °F
ASTM C182
BNZ Materials PA 23 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..