Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.3955 W/m-K @Temperature 800 °C |
2.740 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Chosun Refractories DC-2BS Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.3955 W/m-K @Temperature 800 °C |
2.740 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Chosun Refractories GUN-120L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.3955 W/m-K @Temperature 260 °C |
2.740 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.3955 W/m-K @Temperature 260 °C |
2.740 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Chosun Refractories INCT-140 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |