Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 29.6 W/m-K @Temperature 700 °C |
205 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
International Mold Steel Daido DRM2 Matrix High-Speed Steel This matrix type high speed tool steel is available for warm and cold forging tools where critical performance is required. DRM2 prolongs service life due to its higher hardness and toughness than t.. |
|||
Thermal Conductivity | 29.5 W/m-K @Temperature 199 °C |
205 BTU-in/hr-ft²-°F @Temperature 390 °F |
|
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |
|||
Thermal Conductivity | 29.5 W/m-K @Temperature 200 °C |
205 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili.. |
|||
Thermal Conductivity | 29.6 W/m-K @Temperature 700 °C |
205 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |
|||
Thermal Conductivity | 29.5 W/m-K @Temperature 199 °C |
205 BTU-in/hr-ft²-°F @Temperature 390 °F |
hardened to 310 HB |
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel Cr-Mo alloyed steelP20 Modified offers the following benefits:No hardening risksNo hardening costsTime saving, e.g. no waiting for heat treatmentLower tool cost (e.g. no distortion to rectify)Modifi.. |
|||
Thermal Conductivity | 29.5 W/m-K @Temperature 200 °C |
205 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Assab Steels 618 Plastic Mold Material ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu.. |
|||
Thermal Conductivity | 29.5 W/m-K @Temperature 200 °C |
205 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Assab Steels 718HH Plastic Mold Material IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar.. |