Material Notes:
VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabilityExcellent nitriding propertiesAnd in the processing of plastics by offering:High compressive strengthHigh wear resistanceApplications: Hugh-precision plastic injection molds eg. for the product of camera parts, electronic parts and household itemsCompression molds for all types, eg for plastic containersmolds for elastomersMolds for the production of sealing rings(O-ring seal)Hot running systems
Physical Properties Metric English Comments
Density 7.82 g/cc
0.283 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 30
30
Solution Annealed
38 - 42
38 - 42
Stock Standard
<= 44
<= 44
After Aging
Modulus of Elasticity 210 GPa
30500 ksi
Thermal Properties Metric English Comments
CTE, linear 11.3 µm/m-°C

@Temperature 100 °C
6.28 µin/in-°F

@Temperature 212 °F
12.2 µm/m-°C

@Temperature 200 °C
6.78 µin/in-°F

@Temperature 392 °F
12.8 µm/m-°C

@Temperature 300 °C
7.11 µin/in-°F

@Temperature 572 °F
13.2 µm/m-°C

@Temperature 400 °C
7.33 µin/in-°F

@Temperature 752 °F
13.5 µm/m-°C

@Temperature 500 °C
7.50 µin/in-°F

@Temperature 932 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 25.0 W/m-K

@Temperature 20.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
26.4 W/m-K

@Temperature 100 °C
183 BTU-in/hr-ft²-°F

@Temperature 212 °F
29.5 W/m-K

@Temperature 200 °C
205 BTU-in/hr-ft²-°F

@Temperature 392 °F
31.5 W/m-K

@Temperature 300 °C
219 BTU-in/hr-ft²-°F

@Temperature 572 °F
32.3 W/m-K

@Temperature 400 °C
224 BTU-in/hr-ft²-°F

@Temperature 752 °F
Component Elements Properties Metric English Comments
Aluminum, Al 1.2 %
1.2 %
Carbon, C 0.13 %
0.13 %
Chromium, Cr 0.35 %
0.35 %
Copper, Cu 1.2 %
1.2 %
Iron, Fe 91.32 %
91.32 %
As Balance
Manganese, Mn 2.0 %
2.0 %
Nickel, Ni 3.5 %
3.5 %
Silicon, Si 0.30 %
0.30 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000370 ohm-cm
0.0000370 ohm-cm