Thermal Properties Metric English Comments
Thermal Conductivity 29.5 W/m-K

@Temperature 199 °C
205 BTU-in/hr-ft²-°F

@Temperature 390 °F
EDRO #3 Prehardened Mold Quality P20 Alloy Steel
EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with..
Thermal Conductivity 29.5 W/m-K

@Temperature 200 °C
205 BTU-in/hr-ft²-°F

@Temperature 392 °F
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel
VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili..
Thermal Conductivity 29.5 W/m-K

@Temperature 199 °C
205 BTU-in/hr-ft²-°F

@Temperature 390 °F
hardened to 310 HB
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel
Cr-Mo alloyed steelP20 Modified offers the following benefits:No hardening risksNo hardening costsTime saving, e.g. no waiting for heat treatmentLower tool cost (e.g. no distortion to rectify)Modifi..
Thermal Conductivity 29.5 W/m-K

@Temperature 200 °C
205 BTU-in/hr-ft²-°F

@Temperature 392 °F
Assab Steels 618 Plastic Mold Material
ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu..
Thermal Conductivity 29.5 W/m-K

@Temperature 200 °C
205 BTU-in/hr-ft²-°F

@Temperature 392 °F
Assab Steels 718HH Plastic Mold Material
IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar..