Thermal Properties Metric English Comments
Thermal Conductivity 4.05 - 4.15 W/m-K

@Temperature 600 °C
28.1 - 28.8 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 140 K Dense Refractory Silicon Carbide Castable
This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strengt..
Thermal Conductivity 4.05 - 4.15 W/m-K

@Temperature 1300 °C
28.1 - 28.8 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 140 K Dense Refractory Silicon Carbide Castable
This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strengt..