Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 4.05 - 4.15 W/m-K @Temperature 600 °C |
28.1 - 28.8 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 140 K Dense Refractory Silicon Carbide Castable This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strengt.. |
|||
Thermal Conductivity | 4.05 - 4.15 W/m-K @Temperature 1300 °C |
28.1 - 28.8 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 140 K Dense Refractory Silicon Carbide Castable This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strengt.. |